Swimming Pool Paint | 2K PU Paint
- Suitable to paint all pools (chlorine, saltwater, and mineral) indoors and outdoors
- Properties: UV-resistant, elastic waterproof, highly durable, scratch resistant, and chemical resistant
- Gloss Level: Available in matte or glossy
- Consumption Volume: approx. 0.27fl.oz./sqft per coat. We recommend approximately two coats.
- Processing Temperature: 45°F to 95°F
- Drying Time: Touch Dry/Walkable after 6h at 75°F
- Scope of Delivery: Resin A-component, hardener B-component, and EP Color Paste.
1. Select colour









2. Select quantity
3. Select gloss level

Perfect To Repaint Your Swimming Pool
EPODEX’s Swimming Pool Paint is a budget-friendly solution compared to re-tiling or resurfacing, saving you from costly renovations. Our 2K PU Paint is easy to apply even for beginners. It creates a durable smooth finish that helps prevent surface damage. By smoothing out and reducing micro-cavities, it leaves your pool looking cleaner and easier to maintain.
Instructions For Use
- Ensure the substrate is stable, clean, dry, and free from any substances that may prevent proper adhesion. We recommend sanding to increase adhesion.
- Shake both components individually before use. Then, mix the resin A-component and the hardener B-component in a 3 to 1 mixing ratio (e.g. 45fl.oz resin A-component with 15fl.oz. hardener B-component). Add 5% EP Colour Paste to the resin-hardener mixture to colour it (e.g. 100g (3.5oz) EP Colour Paste to 60fl.oz. resin-hardener mixture).
- Stir through the edge and bottom of the mixing cup as the material will settle there. Ideally, pour into a clean mixing cup and mix again until the mixture is streak-free. This ensures that the resin A-component and hardener B-component are completely mixed together.
- Pour the mixture into a paint tray and apply it thinly with a roller in a criss-cross pattern.
- Let the first coat cure and apply the second coat in the same way. We recommend applying the second coat after min. 3h but not more than 20h.
- We recommend coating the walls before coating the bottom of the pool.
Pro Tip for Flooring:
Do not wear rubber-soled shoes while sanding, cleaning, after cleaning, or during the application of the 2K PU Paint, as rubber microparticles may cause an uneven finish. Rubber-soled shoes can be worn once the second coat of 2K PU Paint is cured. Wait until the 2K PU Paint is walkable (approx. 6 hours) before applying the second coat.


Contractor-Grade Performance
Our Swimming Pool Paint is designed with flexibility to handle thermal expansion and contraction — even through tough winters! When applied properly, it won’t crack or peel once spring arrives. Plus, our 2K PU Paint is UV resistant, so unlike other paints, it won’t yellow or break down under the sun. Resulting in your pool that looks like new and stays that way for years to come. All these benefits make it a smart choice for your next pool upgrade!
reviews
Warning Danger
Highly flammable liquid and vapour. May be fatal if swallowed and enters airways. May cause damage to organs through prolonged or repeated exposure. Causes skin irritation. May cause respiratory irritation. Flammable liquid and vapour. Harmful if inhaled. May cause an allergic skin reaction. May cause drowsiness or dizziness. Contains isocyanates. May produce an allergic reaction. The information on the product label must always be followed.